42CrMo tubería de acero de precisión de aleación laminada en frío
Descripción del producto
Visión general del producto
42CrMo
Chemical Composition(%) | Mechanical Property | |||||||||
C | Si | Mn | S | P | Cr | Ni | Cu | Mo | Yield Strength | Tensile Strength |
( σs ) | ( σb ) | |||||||||
0.38~0.45 | ≤ 0.40 | 0.60~0.90 | ≤0.035 | ≤0.035 | 0.90~1.20 | ≤0.40 | / | 0.15~0.30 | ≥ 930(95)(MPa) |
≥1080(110) |
(MPa) |
Grade and Chemical Composition (%) for ASTM A519 Seamless carbon and Alloy Steel Mechanical pipe |
Grade C Mn P≤ S≤ Si Cr Mo |
1008 ≤0.10 0.30-0.50 0.040 0.050 - - - |
1010 0.08-0.13 0.30-0.60 0.040 0.050 - - - |
1018 0.15-0.20 0.60-0.90 0.040 0.050 - - - |
1020 0.18-0.23 0.30-0.60 0.040 0.050 - - - |
1025 0.22-0.28 0.30-0.60 0.040 0.050 - - - |
1026 0.22-0.28 0.60-0.90 0.040 0.050 - - - |
aisi 4130 0.28-0.33 0.40-0.60 0.040 0.040 0.15-0.35 0.80-1.10 0.15-0.25 |
aisi 4140 0.38-0.43 0.75-1.00 0.040 0.040 0.15-0.35 0.80-1.10 0.15-0.35 |
Mechanical Properties for ASTM A519 Seamless carbon and Alloy Steel Mechanical pipe |
Grade condition tensile pointe Yidld point Elongation |
1020 CW ≥414 ≥483 ≥5% |
SR ≥345 ≥448 ≥10% |
A ≥193 ≥331 ≥30% |
N ≥234 ≥379 ≥22% |
1025 CW ≥448 ≥517 ≥5% |
SR ≥379 ≥483 ≥8% |
A ≥207 ≥365 ≥25% |
N ≥248 ≥379 ≥22% |
aisi 4130 SR ≥586 ≥724 ≥10% |
A ≥379 ≥517 ≥30% |
N ≥414 ≥621 ≥20% |
aisi 4140 SR ≥689 ≥855 ≥10% |
A ≥414 ≥552 ≥25% |
N ≥621 ≥855 ≥20% |